Customization: | Available |
---|---|
CAS No.: | 9016-87-9 |
Source: | ISO/Polyol |
Still deciding? Get samples of US$ 0/kg
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
1)Good liquidity
2)Low thermal conductivity
3)Rapid demoulding
4)Different flame retardant class available
Typical Reactivity Property
Item | Manual Mixing | Low Pressure Foaming Machine | High pressure Foaming Machine |
Cream Time (S) | 12-18 | 10-16 | 8-14 |
Gel Time (S) | 70-90 | 65-80 | 50-75 |
Tack Free Time (S) | 90-120 | 85-110 | 80-110 |
Free Rise Density (Kg/M3) | 23-26 | 23-26 | 22-25 |
TYPICAL PHYSICAL PROPERTIES
Physical Properities | Metric | Value | |
Pen tane | 141B | ||
Thermal Conductivity (Average Temperature 10ºC) | W/(m.K) | 0.021 | 0.0195 |
Compressive Strength | KPa | 130 | 110 |
Dimensional Stability | -30ºC 24h | 1 1.5 |
|
70ºC 24h | |||
Core Density | kg/m3 | ≤38 | ≤35 |
Item | Unit | Specification | Test standard |
Core density | kg/m3 | ≥30 | ASTM D1622-08 |
Thermal conductivity, 10ºC | W/(m.k) | ≤0.019 | ASTM C518-10 |
Compressive strength | kPa | ≥130 | ASTM D1621-10 |
Closed cell content | % | ≥90 | ASTM D6226 |
Water absorb | % | ≤3 | ASTM C209-12 |
Thermal stability, -30-80ºC | % | ≤1.5 | ASTM D2126-09 |
Above Data is for reference only.Actual values vary depending on processing conditions and species.
Preparation
Before using,this polyol has to be mixed very well..